- When high adhesiveness is required, please use
a two-component ink. When selecting an ink, please
consult with the ink manufacturer.
- The basic printing conditions should be set
similar to those of BOPP film printing.
- To avoid poor centering, set the tension at
the lowest possible level.
- Immediately after putting the paper through
the dryer, cool the YUPO® paper
to as close as room temperature as possible.
- Set the printing conditions in such a manner
that the dryer air does not exceed 80°C. Do
not attempt to improve drying efficiency by increasing
the temperature. More effective results will be
achieved by adjusting the wind speed or wind volume.
- For solid patterns, white areas may occasionally
bleed through. Perform a test-print to confirm
beforehand.
|